进口塑胶料
注:请在右边的搜索栏查找产品

PA66 12TA BKB124 含32%矿物,增韧,热稳定

添加时间:2013-11-16  信息来源:http://www.xzslw.com/  作者:苏州希普能塑料

Minlon PA66 12TA BKB124

Minlon® 12TA BKB124 | PA66-I-MD32 MINERAL REINFORCED NYLON RESIN
 
Regional Availability
North America, South and Central America
 
Processing
Injection Moulding
 
Delivery form
Pellets
 
Special characteristics
Heat stabilised or stable to heat
 
Product Text
Common features of Minlon® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness /toughness, good high temperature performance, good chemical resistance, paintability, dimensional stability and low warpage.
 
Grades with improved electrical and flammability properties are available within the Zytel® nylon resin product line. In addition, Minlon® nylon resin is available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses.
 
The good melt stability of Minlon® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.
 
Minlon® nylon resin typically is used in demanding applications in the automotive, electrical, electronic, domestic appliances and construction industries.
 
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection moulding.
 
Injection molding
PREPROCESSING
Drying recommended = Yes
Drying temperature = 80℃
Drying time, dehumidified dryer = 2-4 h
Processing moisture content = <0.2 %
 
PROCESSING
Melt temperature optimum = 295℃
Melt temperature range = 285-305℃
Mould temperature optimum = 100℃
Mould temperature range = 70-120℃
 
PROPERTIES
Mechanical properties dry / cond Unit Test Standard
Tensile Modulus 4800 / 1900 MPa ISO 527-1/-2
Stress at break 78 / 58 MPa ISO 527-1/-2
Strain at break 15 / 40 % ISO 527-1/-2
Charpy impact strength,23℃ 120 / 330 kJ/m² ISO 179/1eU
Charpy impact strength,-30℃ 75 / 80 kJ/m² ISO 179/1eU
Charpy notched impact strength,23℃ 7 / 12 kJ/m² ISO 179/1eA
Charpy notched impact strength,-30℃ 5 / 4 kJ/m² ISO 179/1eA
Charpy notched impact strength,-40℃ 4 / 3 kJ/m² ISO 179/1eA
Thermal properties dry / cond Unit Test Standard
Melting temperature,10℃/min 257 / * ISO 11357-1/-3
Temp. of deflection under load,1.8 MPa 80 / * ISO 75-1/-2
Temp. of deflection under load,0.45 MPa 215 / * ISO 75-1/-2
Other properties dry / cond Unit Test Standard
Density 1380 / - kg/m³ ISO 1183